Cracks
Reasons:
-Performing the last layer of paint to a flexible layer followed by extreme
thermal expansion.
-The last layer paint was performed before the former was not dried well.
Solution:
-The scraping should be done till the proper layer.
-The under layer and last layer should be repeated.
|
|
 |
 |
 |
 |
|
|
 |